✨ New Arrivals Just Dropped!Explore
HomeStore

SikaGrout® 428 FS Fast-Setting Precision Grout - 55 lbs

Product image 1

SikaGrout® 428 FS Fast-Setting Precision Grout - 55 lbs

Fast-Setting And High-Strength, Cementitious Precision Grout. Sikagrout®-428 Fs Ca Is A Cementitious, Non-Shrink And Chloride-Free Precision Grout Powered By Viscocrete® Technology. The Grout Is Designed To Achieve High Early, And Exceptional Ultimate Strengths. As A Precision And Structural Grout, It Can Be Placed At A Minimal Temperature Of +10 °C (+50 °F) And Provides A Substantial Bearing Area.

  • Meets ASTM C1107 requirements
  • Will not stain or rust.
  • Excellent fluidity with sufficient time for placing.
  • Achieves compressive strength in just 12 hours at +23 °C (+73 °F).
  • Exceeds compressive strength of 30 MPa concrete at 24 hours at +23 °C (+73 °F).
  • Provides significant bearing area for transfer of load.

Fast-Setting And High-Strength, Cementitious Precision Grout. Sikagrout®-428 Fs Ca Is A Cementitious, Non-Shrink And Chloride-Free Precision Grout Powered By Viscocrete® Technology. The Grout Is Designed To Achieve High Early, And Exceptional Ultimate Strengths. As A Precision And Structural Grout, It Can Be Placed At A Minimal Temperature Of +10 °C (+50 °F) And Provides A Substantial Bearing Area.

  • Meets ASTM C1107 requirements
  • Will not stain or rust.
  • Excellent fluidity with sufficient time for placing.
  • Achieves compressive strength in just 12 hours at +23 °C (+73 °F).
  • Exceeds compressive strength of 30 MPa concrete at 24 hours at +23 °C (+73 °F).
  • Provides significant bearing area for transfer of load.
$50.43
SikaGrout® 428 FS Fast-Setting Precision Grout - 55 lbs
$50.43

Description

Fast-Setting And High-Strength, Cementitious Precision Grout. Sikagrout®-428 Fs Ca Is A Cementitious, Non-Shrink And Chloride-Free Precision Grout Powered By Viscocrete® Technology. The Grout Is Designed To Achieve High Early, And Exceptional Ultimate Strengths. As A Precision And Structural Grout, It Can Be Placed At A Minimal Temperature Of +10 °C (+50 °F) And Provides A Substantial Bearing Area.

  • Meets ASTM C1107 requirements
  • Will not stain or rust.
  • Excellent fluidity with sufficient time for placing.
  • Achieves compressive strength in just 12 hours at +23 °C (+73 °F).
  • Exceeds compressive strength of 30 MPa concrete at 24 hours at +23 °C (+73 °F).
  • Provides significant bearing area for transfer of load.